HEAT TREATMENT ALLOY BARS

Brand Owner (click to sort) Address Description
HA INDUSTRIES A.M. CASTLE & CO. 1420 Kensington Road, Suite 220 Oak Brook IL 60523 heat treatment of alloy bars and tubes;INDUSTRIES;The stippling in the drawing is for shading purposes.;
HA INDUSTRIES A.M. CASTLE & CO. 1420 Kensington Road, Suite 220 Oak Brook IL 60523 heat treatment of alloy bars and tubes;HA INDUSTRIES;INDUSTRIES;The stippling on the drawing is for shading purposes only.;
 

Where the owner name is not linked, that owner no longer owns the brand

   
Technical Examples
  1. An iron-based alloy comprises 1.5 to 2.5 wt % of C, 0.25 to 4.75 wt % of Ni, and W and V in quantities surrounded by the line L as shown in FIG. 1 of the attached drawings with a balance of Fe and inevitable impurities. The iron-based alloy is obtained by a first heat treatment for applying a solid solution treatment by rapidly cooling the iron-based alloy from a temperature of an austenite forming temperature or more to consequently obtain a mixed matrix comprising a base matrix of martensite and remaining austenite phases and a non-molten carbide, and a second heat treatment for cooling the iron-based alloy after precipitating an MC type carbide within an eutectoid transformation temperature range to consequently precipitate a low carbon content austenite phase.